Hi all,
I'm currently rebuilding a 25HP V-Twin and before I put it all back together I want the case and cylinder cooling fins to be clean and bright aluminium.
So I was wondering if anyone has shot, sand or glass blasted their V-Twin case before and what type of aggregate did you use for best results?
Many thanks.
Neo
I'm currently rebuilding a 25HP V-Twin and before I put it all back together I want the case and cylinder cooling fins to be clean and bright aluminium.
So I was wondering if anyone has shot, sand or glass blasted their V-Twin case before and what type of aggregate did you use for best results?
Many thanks.
Neo